Ion exchange glossary
The words that appear on a resin datasheet, in a water analysis, and in every quotation — defined in one sentence each, the way a plant engineer uses them.
In one line: if two suppliers quote different capacities, check the unit first — mmol/mL is volumetric and sizes the vessel, mmol/g is gravimetric and only compares chemistry.
34 terms
Resin, water and paperwork
Grouped roughly the way a project runs: what the resin is, how it is measured, how it is run, and what travels with it.
| Anion exchange resin | A resin with positively charged fixed groups that exchanges anions such as chloride, sulfate and silicate. Regenerated with sodium hydroxide. |
|---|---|
| Cation exchange resin | A resin with negatively charged fixed groups that exchanges cations such as calcium, magnesium and sodium. Regenerated with brine or acid. |
| Strong acid cation (SAC) | Sulfonic acid resin that removes all cations regardless of the associated anion. Used for softening and as the cation stage of demineralization. |
| Weak acid cation (WAC) | Carboxylic acid resin that removes only the cations bound to alkalinity. High capacity, cheap regeneration, and no effect on neutral salts. |
| Strong base anion (SBA) | Quaternary ammonium resin, Type I or Type II. The only family that removes weakly ionised silica and carbon dioxide. |
| Weak base anion (WBA) | Tertiary amine resin that absorbs strong mineral acids. High capacity and cheap regeneration, but it cannot remove silica or CO2. |
| Gel resin | A dense polymer network swollen with water, with no permanent pores. Higher volumetric capacity; less tolerant of organics and oxidants. |
| Macroporous resin | A bead with a permanent pore structure of 20–100 nm, typically 20–50 m²/g of surface area. Lower capacity, far better fouling resistance and kinetics. |
| Mixed bed | A homogeneous blend of cation and anion resin in one vessel, used to polish demineralised water to below 0.1 µS/cm. |
| Chelating resin | A resin with iminodiacetic or aminophosphonic groups that binds heavy metals by coordination. Selective even in hard water. |
| Adsorbent resin | A macroporous polymer with no functional groups. Removes colour and organics by adsorption, not by ion exchange. |
| Volumetric capacity | Exchange capacity per litre of wet resin, usually in mmol/mL or eq/L. The number to size a vessel with — it tells you how long a bed runs. |
| Gravimetric capacity | Exchange capacity per gram of dry resin, in mmol/g. Useful for comparing chemistry, not for sizing a vessel. |
| Moisture content | Water held inside a fully swollen bead, as a percentage of wet weight. A rise against the original certificate suggests oxidation or fouling. |
| Bulk density | Mass of wet resin per unit volume as packed, typically 650–850 g/L. Used to convert a resin volume into a shipping weight and bag count. |
| Effective bead size | The sieve size at which 10 % of the beads are smaller, in mm. 0.40–0.70 mm covers most softening and demineralization. |
| Uniformity coefficient | The ratio of the 60 % to the 10 % bead size. At 1.60 or below, the bed classifies cleanly and the pressure drop stays predictable. |
| Crosslink (DVB) | Divinylbenzene content, written in the model number — 001×7 contains 7 % DVB. More crosslink means lower moisture, slower kinetics and less swelling. |
| Swelling | Volume change when the resin changes ionic form, for example Na+ to H+. Large swelling needs freeboard or the bed lifts the distributor. |
| EBCT | Empty bed contact time — bed volume divided by flow rate. Softening 2–6 minutes, demineralization 2–5 minutes, mixed beds 1–2 minutes. |
| Service flow rate | The flow per unit of bed cross-section, in m/h or bed volumes per hour. It sets the pressure drop and the risk of channeling. |
| Breakthrough | The point at which the ion being removed first appears in the outlet. Run length is measured to breakthrough, not to exhaustion. |
| Leakage | Ions still present in the outlet after regeneration. It follows the regeneration dose and the bed depth, not the resin quantity. |
| Regeneration | Restoring the exchange sites with brine, acid or caustic. Efficiency is the fraction of the regenerant actually used by the bed. |
| Brine | Sodium chloride solution used to regenerate sodium-cycle cation resin, typically 8–10 % and 100–150 g per litre of resin. |
| Attrition | Loss of whole beads through mechanical wear, osmotic shock and thermal cycling. Measured as an attrition or whole-bead rate, not as capacity. |
| Fines | Fragments smaller than the specified bead size, produced by attrition. They raise pressure drop and blind downstream filters. |
| Hardness | Calcium and magnesium content, expressed as mg/L CaCO3 or meq/L. 1 meq/L equals 50 mg/L as CaCO3. |
| TDS | Total dissolved solids, mg/L. Above roughly 1 000 mg/L a softening bed is usually the wrong tool and demineralization is cheaper overall. |
| Silica | SiO2 in the feed, mg/L. Above 0.5 mg/L only strong base Type I resin removes it, and only when regenerated with warm caustic. |
| meq/L and mmol/L | For a monovalent ion, 1 meq/L equals 1 mmol/L. For calcium, 1 mmol/L equals 2 meq/L — check which unit the lab reported. |
| COA | Certificate of analysis — the batch-specific test report that accompanies a shipment: capacity, moisture, bead size, density, attrition. |
| SDS | Safety data sheet, 16 sections in GHS format. Ion exchange resin is not regulated as dangerous goods for sea transport. |
| IMDG | The International Maritime Dangerous Goods code. Resin is not subject to it, which is why shipments move as general cargo. |
Units that catch people out
- 1 meq/L = 50 mg/L as CaCO3
- For calcium, 1 mmol/L = 2 meq/L
- 1 mmol/mL = 1 eq/L = 1 000 eq/m³
- 1 ppm ≈ 1 mg/L in dilute aqueous solution
Reviewed by the MAISEN technical team · last updated · corrections and additions welcome by email.